Mechanical profiling
Moisture mitigation
Resin build leveling
Topcoat calibration
Planetary diamond grinders and captive shot-blasters strip weak laitance and contaminants, opening concrete capillary pores to achieve a certified CSP 3 to 5 anchor profile.
Calcium chloride and relative humidity probe testing measure vapor emission rates. Slabs exceeding threshold limits receive a dedicated 100% solids epoxy moisture vapor barrier.
High-tensile body coats and graded silica broadcasts establish specified millimetre thickness, structural density, and uniform load distribution across expansion joints.
Aliphatic polyurethane coats lock the matrix against aggressive chemicals, UV exposure, and abrasive rubber-wheel traffic across high-traffic manufacturing corridors.
Mechanical tolerances
12,000 PSI
compressive strength
85 Shore D
surface hardness
>400 PSI
substrate tensile bond
0.1 g
Taber abrasion loss
Schedule slab evaluation
On-site core inspection, hardness verification, and moisture vapor emission testing for industrial plants.